留言板

尊敬的读者、作者、审稿人, 关于本刊的投稿、审稿、编辑和出版的任何问题, 您可以本页添加留言。我们将尽快给您答复。谢谢您的支持!

姓名
邮箱
手机号码
标题
留言内容
验证码

KDP晶体表面残留磁流变抛光液清洗技术研究

李晓媛 高伟 田东 董会 吉方 王超

李晓媛, 高伟, 田东, 董会, 吉方, 王超. KDP晶体表面残留磁流变抛光液清洗技术研究[J]. 红外与激光工程, 2018, 47(S1): 132-137. doi: 10.3788/IRLA201847.S120006
引用本文: 李晓媛, 高伟, 田东, 董会, 吉方, 王超. KDP晶体表面残留磁流变抛光液清洗技术研究[J]. 红外与激光工程, 2018, 47(S1): 132-137. doi: 10.3788/IRLA201847.S120006
Li Xiaoyuan, Gao Wei, Tian Dong, Dong Hui, Ji Fang, Wang Chao. Study on cleaning of residual from magnetorheological finishing(MRF) of potassium dihydrogen phosphate(KDP) crystal surface[J]. Infrared and Laser Engineering, 2018, 47(S1): 132-137. doi: 10.3788/IRLA201847.S120006
Citation: Li Xiaoyuan, Gao Wei, Tian Dong, Dong Hui, Ji Fang, Wang Chao. Study on cleaning of residual from magnetorheological finishing(MRF) of potassium dihydrogen phosphate(KDP) crystal surface[J]. Infrared and Laser Engineering, 2018, 47(S1): 132-137. doi: 10.3788/IRLA201847.S120006

KDP晶体表面残留磁流变抛光液清洗技术研究

doi: 10.3788/IRLA201847.S120006
基金项目: 

国家自然科学基金(51575501,51202228);科学挑战专题(JCKY2016212A506-0503);中国工程物理研究院发展基金(2015B0203030)

详细信息
    作者简介:

    李晓媛(1987-),女,工程师,硕士,主要从事光学元件超精密加工及后处理方面的研究。Email:lxy20056482@126.com

  • 中图分类号: TH161

Study on cleaning of residual from magnetorheological finishing(MRF) of potassium dihydrogen phosphate(KDP) crystal surface

  • 摘要: 磷酸二氢钾(KDP)晶体是一种非常优良的非线性光学晶体材料,在强激光系统中有着重要应用。但其理化性质特殊,加工高表面质量的元件难度很大。目前研究认为磁流变抛光技术能够获得高精度的KDP晶体表面,但是该加工过程带入的表面残留如不清除,会大大降低元件的性能。提出了一种针对磁流变抛光后续的KDP的清洗技术,设计了含水活性清洗液,结合超高频超声作用共同去除KDP表面残留。光学显微镜和白光干涉仪分析表明,该技术较好地去除了表面残留,并且晶体表面粗糙度有所降低。拉曼光谱和激光干涉仪测试表明,清洗前后KDP表面化学结构和面形精度一致。该研究获得了较为满意的结果,说明该方法是一种有应用前景的KDP超精密清洗方法。
  • [1] Fuchs B A, Hed P P, Baker P C, et al. Fine diamond turning of potassium dihydrogen phosphate crystals[J], Applied Optics, 1986, 25(11):1733-1735.
    [2] Chen Dongsheng, Ji Fang, Chen Hua, et al. Research on the low speed stability control technology of fly-cutting machine for KDP crystals[C]//7th International Symposium on Advanced Optical Manufacturing and Testing Technologies:Advanced Optical Manufacturing Technologies, 2014, 92810P.
    [3] Wang Shenglai, Ding Jianxu. Research progress of KDP crystal[J]. Journal of Synthetic Crystals, 2012, 41(S1):179-183. (in Chinese)
    [4] Shao Jianda, Dai Yifan, Xu Qiao. Progress on optical components for ICF laser facility[J]. Optics and Precision Engineering, 2016, 24(12):2889-2895. (in Chinese)
    [5] Gao Wei, Wang Lili, Tian Lunfu, et al. Novel abrasive-free jet polishing mechanism for potassium dihydrogen phosphate (KDP) crystal[J]. Optical Materials Express, 2018, 8(4):1012-1024.
    [6] Ji Fang, Xu Min, Wang Baorui, et al. Preparation of methoxyl poly(ethylene glycol) (MPEG)-coatedcarbonyl iron particles (CIPs) and their application in potassiumdihydrogen phosphate(KDP) magnetorheological finishing(MRF)[J]. Applied Surface Science, 2015, 353(1):723-727.
    [7] Wang Fengrui, Li Qingzhi, Guo Decheng, et al. Laser pretreatment parameters optimization of KDP crystal[J].Infrared and Laser Engineering, 2017, 46(3):0321005. (in Chinese)
    [8] Ji Fang, Xu Min, Wang Chao, et al. The magnetorheological finishing (MRF) of potassium dihydrogen phosphate (KDP)Crystal with Fe3O4 nanoparticles[J]. Nanoscale Research Letters, 2016, 11:79.
    [9] Wang Beng, Wu Dongjiang, Gao Hang, et al. Influence of cleaning method on quality of KDP crystal polished surface[J]. Journal of Synthetic Crystals, 2009, 38(2):525-534.(in Chinese)
    [10] Yuan Zheng, Dai Yifan, Xie Xuhui, et al. Cleaning of iron powders embedded into the surface of KDP crystal by ion beam figuring[J]. Journal of Synthetic Crystals, 2013, 42(4):582-586. (in Chinese)
    [11] Gao Xiang, Qiu Rong, Zhou Guorui, et al. Effect of subsurface impurities of fused silica on laser induced damage probability[J]. Infrared and Laser Engineering, 2017, 46(4):0106002. (in Chinese)
    [12] Tayyab Suratwala, William Steele, Michael Feit, et al. Mechanism and simulation of removal rate and surface roughness during optical polishing of glasses[J]. Journal of the American Ceramic Society, 2016, 99(6):1974-1984.
    [13] Li Yaguo, Zheng Nan, Li Haibo. Morphology and distribution of subsurface damage in optical fused silica parts:Bound-abrasive grinding[J]. Applied Surface Science, 2011, 257(6):2066-2073.
    [14] Chen Yuchuan, Gao Hang, Wang Xu. Investigation on the cleaning of KDP ultra-precision surface polished with micro water dissolution machining principle[J]. Science China, 2017, 60(1):27-35. (in Chinese)
    [15] Wang Biling. Abrasive-free water-dissolution polishing and processing mechanism for KDP crystal[D]. Dalian:Dalian University of Technology, 2010.(in Chinese)
  • [1] 王蔚, 王孝宇, 刘伟军, 邢飞, 王静.  光斑搭接率对GH3030合金表面积碳及氧化物清洗质量的影响 . 红外与激光工程, 2023, 52(2): 20220164-1-20220164-10. doi: 10.3788/IRLA20220164
    [2] 郭斌, 徐杰, 苏轩.  大能量高重频脉冲激光智能清洗技术与装备 (特邀) . 红外与激光工程, 2023, 52(2): 20230073-1-20230073-4. doi: 10.3788/IRLA20230073
    [3] 江宇宏, 何玉洋, 符永宏, 纪敬虎, 佟艳群.  激光清洗技术规模化应用发展现状(特邀) . 红外与激光工程, 2023, 52(2): 20220753-1-20220753-8. doi: 10.3788/IRLA20220753
    [4] 刘丽飒, 林学春, 宋峰.  激光器工程化与清洗应用中的技术突破 (特邀) . 红外与激光工程, 2023, 52(2): 20230049-1-20230049-5. doi: 10.3788/IRLA20230049
    [5] 郭嘉伟, 蔡和, 韩聚洪, 罗清, 杨蛟, 安国斐, 宋迪, 王佳琪, 王浟.  基于热烧蚀效应的激光清洗仿真模型研究(特邀) . 红外与激光工程, 2023, 52(2): 20220779-1-20220779-9. doi: 10.3788/IRLA20220779
    [6] 李世杰, 张丽君, 何佳, 何长涛, 韩敬华.  声光复合的激光清洗飞机蒙皮实时监测 (特邀) . 红外与激光工程, 2023, 52(2): 20220821-1-20220821-10. doi: 10.3788/IRLA20220821
    [7] 张月来, 龙维峰, 姚杞, 林吉, 刘泽辉, 刘博文.  铝合金车体焊接同步激光清洗技术研究 (特邀) . 红外与激光工程, 2023, 52(2): 20220534-1-20220534-8. doi: 10.3788/IRLA20220534
    [8] 张若楠, 韦朋余, 郭鑫, 陈小平, 黄旭峰, 王连, 王若烨.  EH36钢激光清洗参数优化与表面性能评估 . 红外与激光工程, 2023, 52(2): 20220155-1-20220155-9. doi: 10.3788/IRLA20220155
    [9] 佟艳群, 陆蒋毅, 叶云霞, 符永宏, 蒋滨, 丁柳馨, 任旭东.  玻璃表面微颗粒的激光清洗研究(特邀) . 红外与激光工程, 2023, 52(2): 20220782-1-20220782-9. doi: 10.3788/IRLA20220782
    [10] 李悦, 吴卓颐, 储德谱, 杨火木, 邓国亮, 周寿桓.  激光清洗监测技术研究进展(特邀) . 红外与激光工程, 2023, 52(2): 20220784-1-20220784-19. doi: 10.3788/IRLA20220784
    [11] 宋峰, 陈铭军, 陈晅, 赵泽家, 刘鑫, 姚建铨.  激光清洗研究综述(特邀) . 红外与激光工程, 2023, 52(2): 20220835-1-20220835-22. doi: 10.3788/IRLA20220835
    [12] 王静轩, 张继花, 李玉海, 廖威, 王成程, 袁晓东.  可在线应用的大口径溶胶-凝胶膜光学元件激光清洗工艺研究(特邀) . 红外与激光工程, 2023, 52(2): 20220739-1-20220739-9. doi: 10.3788/IRLA20220739
    [13] 王凯, 李多生, 叶寅, 罗军明, 龙思海, 官冀原, 谢非彤, 姜苏航, 王明娣, 吴宁.  航空铝合金表面涂层无损激光清洗研究 . 红外与激光工程, 2022, 51(12): 20210936-1-20210936-9. doi: 10.3788/IRLA20210936
    [14] 薛亚飞, 王巍, 王学锋, 王军龙, 李广, 高文焱, 李本海, 李凯.  38CrMoAl材料表面污染物激光清洗技术 . 红外与激光工程, 2018, 47(7): 706004-0706004(7). doi: 10.3788/IRLA201847.0706004
    [15] 王凤蕊, 李青芝, 郭德成, 黄进, 耿锋.  KDP晶体激光预处理参数的优化 . 红外与激光工程, 2017, 46(3): 321005-0321005(6). doi: 10.3788/IRLA201746.0321005
    [16] 常青, 李亚蕾.  不同激光脉冲作用下ZnS晶体非线性光学特性 . 红外与激光工程, 2015, 44(5): 1534-1538.
    [17] 乌日娜, 李勇, 闫彬, 岱钦, 于涛, 徐送宁.  液晶分子取向对一维光学多层膜光子晶体透射谱的影响 . 红外与激光工程, 2013, 42(3): 738-741.
    [18] 陈哲, 吕锋, 葛菁华, 张军, 余健辉, 林宏奂, 隋展.  增强偏振态二维无序分布特性的光学晶体退偏器 . 红外与激光工程, 2013, 42(5): 1258-1264.
    [19] 薛永宏, 安玮, 张涛, 张寅生.  采用扩展MRF的红外目标自适应检测方法 . 红外与激光工程, 2013, 42(8): 2288-2293.
    [20] 沈华, 张英聪, 朱日宏.  基于光热位移原理的KDP晶体光吸收系数干涉测量方法的数学模型及结构参数优化 . 红外与激光工程, 2013, 42(12): 3353-3357.
  • 加载中
计量
  • 文章访问数:  477
  • HTML全文浏览量:  114
  • PDF下载量:  44
  • 被引次数: 0
出版历程
  • 收稿日期:  2018-02-05
  • 修回日期:  2018-05-03
  • 刊出日期:  2018-06-25

KDP晶体表面残留磁流变抛光液清洗技术研究

doi: 10.3788/IRLA201847.S120006
    作者简介:

    李晓媛(1987-),女,工程师,硕士,主要从事光学元件超精密加工及后处理方面的研究。Email:lxy20056482@126.com

基金项目:

国家自然科学基金(51575501,51202228);科学挑战专题(JCKY2016212A506-0503);中国工程物理研究院发展基金(2015B0203030)

  • 中图分类号: TH161

摘要: 磷酸二氢钾(KDP)晶体是一种非常优良的非线性光学晶体材料,在强激光系统中有着重要应用。但其理化性质特殊,加工高表面质量的元件难度很大。目前研究认为磁流变抛光技术能够获得高精度的KDP晶体表面,但是该加工过程带入的表面残留如不清除,会大大降低元件的性能。提出了一种针对磁流变抛光后续的KDP的清洗技术,设计了含水活性清洗液,结合超高频超声作用共同去除KDP表面残留。光学显微镜和白光干涉仪分析表明,该技术较好地去除了表面残留,并且晶体表面粗糙度有所降低。拉曼光谱和激光干涉仪测试表明,清洗前后KDP表面化学结构和面形精度一致。该研究获得了较为满意的结果,说明该方法是一种有应用前景的KDP超精密清洗方法。